Difference between revisions of "Fiberglass"
From Advance Coatings Wiki
Jump to navigationJump to search(2 intermediate revisions by the same user not shown) | |||
Line 1: | Line 1: | ||
We currently sell fiberglass by the roll. Our stock varies, so please ask us what we have available at a given time. We are likely to have the basics (matte, woven roving, and cloth tape). | We currently sell fiberglass by the roll. Our stock varies, so please ask us what we have available at a given time. We are likely to have the basics (matte, woven roving, and cloth tape). | ||
+ | |||
+ | ==Tips== | ||
+ | ===The resin should fully soak through the fiberglass=== | ||
+ | A mistake that can be made when using fiberglass is to not get the resin through all of the fibers. What happens then is that the surface glass gets coated in resin, yet the under layers of glass threads remain unsoaked. This will result in a weaker end product, and is to be avoided. To see a microscope picture of this mistake in practice, please see [[SEM_Images#3210_LVP]] | ||
+ | |||
==Images== | ==Images== | ||
<gallery> | <gallery> | ||
Line 12: | Line 17: | ||
File:Fiberglass matte2.jpg|200px|thumb|| | File:Fiberglass matte2.jpg|200px|thumb|| | ||
</gallery> | </gallery> | ||
+ | |||
+ | |||
+ | [[Category:Products]] |
Latest revision as of 06:44, 5 September 2023
We currently sell fiberglass by the roll. Our stock varies, so please ask us what we have available at a given time. We are likely to have the basics (matte, woven roving, and cloth tape).
Tips
The resin should fully soak through the fiberglass
A mistake that can be made when using fiberglass is to not get the resin through all of the fibers. What happens then is that the surface glass gets coated in resin, yet the under layers of glass threads remain unsoaked. This will result in a weaker end product, and is to be avoided. To see a microscope picture of this mistake in practice, please see SEM_Images#3210_LVP